The images shown are merely indicative and represent an example of the type of stone, before any order should always be requested a photo or sample of the desired variety.
Physical and mechanical properties
Flexural resistence under centered load: | 12.7MPa |
Flexural resistence under centered load after testing freeze / unfreeze (48 cycles): | 12.2MPa |
Resistance to Anchorage: | 228 Kg |
Determination of Water Absorption at Normal Atmospheric Pressure: | 4.4% |
Determination of Volumetric Weight: | 2340 Kg/m² |
Determination of Porosity: | 9.8% |